Abstract

The as-spun fibers, which be produced by dry spinning technique, were treated with methanol solution. The results showed that the morphology, structure and mechanical properties of the as-spun fibers had changed. Before methanol treatment,the as-spun fiber had a smooth surface, after methanol treatment, the fiber exhibited rough surface and banded features along the fiber axis. The structure of the as-spun fibers changed from random-coil or silk I conformation to silk II conformation and the breaking intensity of the as-spun fibers were improved after methanol treatment. Compared with degummed silk fibers, the fibers treated with methanol had higher module, but the breaking elongation was lower, the fibers were still brittle.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.