Abstract
The adsorptive characteristics of biochar produced from garden green waste (S-char) and a mixture of food waste and garden green waste (FS-char) were investigated. Adsorption of Cu2+, Zn2+, and Mn2+ onto the two biochars reached equilibrium within 48 hours. The metal adsorption was effectively described by the pseudo-second-order kinetic and Freundlich isotherm models which suggest heterogeneous chemisorption. The initial solution pH influenced adsorption of Zn2+ and Mn2+ but not of Cu2+. Simulation via a surface complexation model showed that the fraction of XOCu+ adsorbed onto biochar was increased with increasing pH until it reached the adsorption maximum at pH 8.5, while the endpoint for the maximum of XOMn+ was higher than pH 12.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.