Abstract

Recycling of samarium–cobalt (SmCo) magnets is essential due to the limited resources of the mentioned metals and their high economic importance. The ionic liquid (IL) trihexyltetradecylphosphonium trichloride, [P666,14][Cl3], which can safely store chlorine gas in the form of the trichloride anion, was used as an oxidizing solvent for the recovery of metals from spent SmCo magnets. The dissolution was studied considering various mixtures of the ILs [P666,14][Cl3] and [P666,14]Cl, solid-to-liquid ratios and different temperatures. The results showed that the maximum capacity of [P666,14][Cl3] for SmCo magnets was 71 ± 1 mg/g of [P666,14][Cl3], in the presence of an extra source of coordinating chloride ions. The maximum loading of the IL could be reached within 3 h at 50 °C. Four stripping steps effectively removed all metals from the loaded IL, where sodium chloride solution (3 mol L–1), twice water and ammonia solution (3 mol L–1) were used consecutively as the stripping solvents. The regenerated IL showed a similar dissolution performance as fresh IL. Oxidative dissolution of metals in trichloride ILs is easily transferable to the recycling of valuable metals from other end-of-life products such as neodymium–iron–boron magnets and nickel metal hydride batteries.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.