Abstract
We report on the successful implementation of interconnects with metal–organic chemical vapor-deposited copper using dual damascene technology. The average resistances of the Kelvin vias and via chains (with a via diameter of 0.28 μm) are 0.62 and 0.72 Ω, respectively. The average line–line leakage current measured at a field of 4500 V/cm at room temperature is about 10 −10 A. It does not increase significantly with the applied electrical field up to about 2.5 MV/cm. These data meet the industrial standards for copper interconnects in the deep submicron integrated circuits and can be improved further by optimizing the ionized metal plasma flash copper.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.