Abstract

The effects of metal alkoxide type and relative humidity on the durability of alkoxide-primed, adhesively bonded steel wedge crack specimens have been determined. Aluminum tri-secbutoxide, aluminum tri-tert-butoxide, tetrabutyl orthosilicate, and titanium(IV ) butoxide were used as alkoxide primers. Grit-blasted, acetone-rinsed mild steel adherends were the substrates bonded with epoxy and polyethersulfone. The two aluminum alkoxides significantly enhanced the durability of the adhesively bonded steel, while the titanium alkoxide showed no improvement in durability over a nonprimed control. The silicon alkoxide-primed samples gave an intermediate response. The failure plane in the adhesively bonded samples varied with the relative humidity during the priming process.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.