Abstract
Abstract The melt drawability including melt strength (MS) and stretching ratio (V) of the neat low-density polyethylene (LDPE) and the LDPE composites loaded with a nanometer zinc oxide (nano-ZnO) were measured using a melt spinning method in capillary extruding temperature varied from 160 to 200 °C and within capillary flow rate range from 9 to 36 mm/s. It was found that the stretching ratio of the neat LDPE and the LDPE/nano-ZnO composites reduced with an increase of capillary flow rate while the V added with in a rise of capillary temperature. The melt strength of the neat LDPE and the LDPE/nano-ZnO composites enlarged with raising capillary flow speed; the MS reduced with an addition of capillary temperature. In addition, the dependence of the MS of the composites on the capillary temperature approximately accorded the Arrhenius expression.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Advanced Industrial and Engineering Polymer Research
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.