Abstract

Solid electrolytes with high ionic conductivity, high formability, and high electrochemical properties are required to improve the performance of all-solid-state sodium batteries. In this study, we focus on a combination of Na2.88Sb0.88W0.12S4 and NaI for preparing composite electrolytes Na2.88Sb0.88W0.12S4·xNaI, and investigate their crystal structures, microstructures, and electrochemical properties. NaI is uniformly dispersed in the composites without forming a solid solution with Na2.88Sb0.88W0.12S4. Na2.88Sb0.88W0.12S4·0.50NaI shows a high ionic conductivity of 3.6 × 10−2 S cm−1 after sintering at 275 °C for only 1.5 h. The charge-discharge characteristics of all-solid-state cells using the Na2.88Sb0.88W0.12S4·xNaI composite are also improved.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.