Abstract

Abstract The britholites have gained a great interest thanks to their potential applications as matrices for the confinement of the byproducts in the nuclear industry such as minor actinides and long-lived fission products. However, the preparation of britholites requires high temperatures, above 1200 °C. In this work, we strive to prepare these kinds of compounds by a mechanochemical synthesis at room temperature from the starting materials SrF 2 , SrCO 3 , Sr 2 P 2 O 7 , La 2 O 3 and SiO 2 using a planetary ball mill. The obtained results showed that the prepared products were carbonated apatites and the corresponding powders contained some unreacted silica and lanthana. To obtain pure britholites, a heat-treatment at 1100 °C was required. The mechanism involved in the different steps of the reaction is discussed in this paper. The obtained results suggest that the use of raw materials containing no carbonate is expected to directly lead to pure britholites by appropriate milling at room temperature.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call