Forged components of ferritic steel are protected by a welded austenitic clad. intergranular cracking can take piace in the ferritic phase close to the ferritic austenitic interface. After developing a fabrication technique for these cracks, the formation conditions are studied. Auger electron spectroscopy investigations of specimens containing a real crack opened inside the vacuum chamber are used for interpretation. Sulphur segregations embrittle the grain boundaries which are separated by different dilatations of the clad and the base metal during the postweld heat treatment.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.