Abstract

Metallic Ni surface was examined as a catalyst for the hydrazine hydrate oxidation reaction (HHOR) by cyclic voltammetry, chronoamperometry, and online differential electrochemical mass-spectrometry (DEMS). It was found that N2 is the sole gaseous product formed during the HHOR on Ni and 4 electrons are transferred in the process, which corresponds to a complete oxidation of the hydrazine molecule. The mechanism of the HHOR on the Ni surface involves OH− and adsorbed OHads intermediate, the latter improving the rate of the HHOR. Ni catalysts were found to be poisoned during the HHOR, the extent of poisoning depending on the number of surface sites, hydrazine concentration, and the α-Ni(OH)2 coverage. Ex situ X-ray photoelectron spectroscopy (XPS) measurements were performed to characterize the species poisoning Ni surface.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.