Abstract

In this study, a type of fly ash and iron tailing powder were used as a binary supplementary cementitious material (SCM) and two different mechanically activated procedures, named coalescent activation and separated activation, were carried out to improve the pozzolanic reactivity. Then, three binary supplementary cementitious materials were used to replace 30 wt% of ordinary Portland cement to develop cemented mortars, and the compressive strength, hydration products, and micro-structure were studied. The experimental results indicated that the activated supplementary cementitious materials increased the compressive strengths of the mortars by 5.4% and 13.2%, negligibly changed the hydration product types, and impacted the quantity only. The application of SCMs also prolonged the setting time and decreased the hydration rate, profiting the application. Simultaneously, the micro-pore structure was ameliorated, and the porosity decreased. Therefore, comprehensively considering the improved mechanical behavior and inexpensive cost, the activated binary SCM can be considered an ecological and economical admixture, especially for the coalescent activation procedure.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.