Abstract

A series of post-crosslinked resins were synthesized from macroporous chloromethylated styrene-divinylbenzene copolymer by controlling post-crosslinked reaction conditions. Adsorption study towards aniline showed that the three resins, ST-DVB-WH5, ST-DVB-WH6, and ST-DVB-WH7, prepared at different temperatures, and which had nearly identical static adsorption capacity, displayed great disparity in kinetic behavior. The rate constant of ST-DVB-WH7 by the pseudo-first-order model was 1.50 and 1.19 times higher than that of ST-DVB-WH5 and ST-DVB-ST-DVB-WH6. Further analysis of the diffusion model showed that the three resins exhibited different diffusion rates due to the difference in oxygen content and pore structure of each resin. The results showed that the adsorption capacity was mainly decided by the pore volume within 1.14 and 3.42 nm and the adsorption rate was mainly decided by the oxygen content of the resin. In addition, as the best synthetic resin for aniline adsorption, the equilibrium adsorption capacity of ST-DVB-WH7 was 1.57 times and 1.44 times higher than that of H-103 and NKA-II, respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.