Abstract

Porous aerogel materials have advantages of a low density, low thermal conductivity and high porosity, and they have broad application prospects in heat insulation and building energy conservation. However, aerogel materials usually exhibit poor mechanical properties. Single-component aerogels are less likely to possess a good thermal stability and mechanical properties. It is necessary to prepare multiple-composite aerogels by reinforcement to meet practical application needs. In this experiment, a simple preparation method for polyvinyl alcohol (PVA)–graphene (GA)–nanocellulose (CNF) ternary composite aerogels was proposed. This is also the first time to prepare ternary composite aerogels by mixing graphene, nanocellulose and polyvinyl alcohol. A GA–CNF hydrogel was prepared by a one-step hydrothermal method, and soaked in PVA solution for 48 h to obtain a PVA–GA–CNF hydrogel. PVA–GA–CNF aerogels were prepared by freeze drying. The ternary composite aerogel has advantages of excellent mechanical properties, a low thermal conductivity and an improved thermal stability, because strong hydrogen bonds form between the PVA, GA and CNF. The composite aerogels were characterized by scanning electron microscopy, Fourier transform infrared spectroscopy, X-ray diffractometry, Brunauer–Emmett–Teller analysis, dynamic thermal analysis, thermogravimetry and thermal constant analysis to characterize the properties of the ternary composite aerogels. The lightweight, low-density and porous PVA–GA–CNF composite aerogels withstood 628 times their mass. The thermal conductivity of the composite aerogels was 0.044 ± 0.005 W/mK at room temperature and 0.045 ± 0.005 W/mK at 70 °C. This solid, low thermal conductivity and good thermal stability PVA–GA–CNF ternary composite aerogel has potential application in thermal insulation.

Highlights

  • IntroductionAerogel materials have structural characteristics of a low density, high specific surface area, high porosity and high pore volume [1]

  • Introduction published maps and institutional affilAerogel materials have structural characteristics of a low density, high specific surface area, high porosity and high pore volume [1]

  • A preparation method for ternary composite aerogels composed of polyvinyl alcohol (PVA), GA and CNF

Read more

Summary

Introduction

Aerogel materials have structural characteristics of a low density, high specific surface area, high porosity and high pore volume [1]. Aerogel materials have broad application prospects in many fields, such as thermal insulation, adsorption and separation, biomedicine, photoelectrocatalysis, energy storage conversion, sound absorption and insulation, and high-energy particle capture [5]. These properties have attracted widespread attention in scientific research, production, and design, and have become a key research field in material science [6]. The average aerogel pore size is ~20 nm, which is much smaller than the average free path iations

Methods
Results
Conclusion