Abstract

Based on the traditional Mn13, the new cast high manganese steel was prepared by adding different Cr, Mo, B, and Re elements in the composition. Its microstructure, mechanical properties, and wear quantity of surface were investigated. Results show that after water toughening, the pearlite dissolved and a few linear carbides were kept at the boundary of grains in the microstructure. All of the hardness was more than 220 HB, impact toughness reached or exceeded 140 J/cm2, and ultimate tensile strength was 753 MPa. The lowest abrasive wear quantity was 0.02 g. The newly cast high manganese steel was applied to produce breaking teeth casting of the crusher. Velocity and temperature fields were simulated to predict some defects during the mold filling and solidification process with finite element software for 4 foundry processes. The optimal technological parameter was adapted to make breaking teeth components.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.