Abstract

This paper deals with the mechanical properties and degree of swelling (DS) of starch/PVA blend film with the functional groups i.e., hydroxyl and carboxyl group, of additives. Starch/PVA blend films were prepared by using the mixing process. Glycerol (GL) with 3 hydroxyl group, sorbitol (SO) with 6 hydroxyl group, succinic acid (SA) with 2 carboxyl group, malic acid (MA) with 1 hydroxyl and 2 carboxyl group, tartaric acid (TA) with 2 hydroxyl and 2 carboxyl group and citric acid (CA) with 1 hydroxyl and 3 carboxyl group were used as additives. The results of measured tensile strength (TS) and elongation (%E) verified that both hydroxyl and carboxyl group as a functional groups increased the flexibility and strength of the film. Values of DS for GL-added and SA-added films were low. However, DS values of the films added MA, TA or CA with both hydroxyl and carboxyl group were comparatively high. When the film was dried at low temperature, the properties of the films were evidently improved. The reason is probably because the hydrogen bonding was activated at low temperature.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call