Abstract

In order to replace Ti-Ni shape memory alloys, new biomedical shape memory alloys have been developed which are composed of beta titanium and nontoxic elements only. In this paper, experimental results of mechanical and shape memory properties are reported for the Ni-free Ti-18mol%Nb shape memory alloys containing 3mol% of 13-group and 14-group ternary elements in the periodic table. The ternary elements selected are Al, Ga, In, Ge and Sn. It was found that the solution treated alloys exhibit good shape memory effect but almost no pseudoelasticity at room temperature. Ultimate tensile strength and elongation to failure at room temperature are ranged from 250 to 710MPa and from 13 to 21%, respectively, depending on the kind of ternary elements. Effect of solution hardening on strength is discussed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.