Abstract

Objective: To clarify mechanical properties of 14 superelastic NiTi orthodontic wires by three-point bending tests. Materials and Methods: The three-point bending test was conducted with a midspan deflection rate of 5 mm/min under constant temperature range 36±1°C. Wires were deflected to 3.1 mm. All data were recorded during the unloading process at deflections 3, 2, 1 and 0.5 mm. to simulate the force a wire exerts as a tooth is moved into the dental arch from a position of malocclusion. Results: The delivered forces changed slightly when the deflection varied during loading and unloading. Sentalloy wire applied the lowest continuous force. Conclusions: Commercial wires may not behave similarly due to minor differences in the production process, and force varies greatly from brand to brand. NiTi wire brands must be selected carefully considering the severity of malocclusion and stage of orthodontic treatment.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.