Abstract

Powder reuse can reduce the material costs associated with additive manufacturing (AM). Powder reuse is posited to have immediate cost savings, such as for the orthopedic industry. However, process deviation in the medical device industry requires that both material and part quality be quantitatively assessed with respect to reuse. The ultimate tensile strength (UTS) and elongation at break (EaB) were measured from selective laser sintered nylon specimens printed with recovered build chamber powder reused 1, 4 and 8 times. Using a design of experiment approach, build temperature, layer thickness, laser speed and laser power were confirmed to influence UTS. Statistical analysis revealed that location in the bed influences UTS, but not EaB. UTS decreased significantly between Reuse 1 and 4, but not between Reuse 4 and 8, whereas EaB (evaluated with the non-parametric Friedman’s test) was unaffected for both pairwise comparisons (p>0.05). A 50-50 blend demonstrated a diminished effect on UTS and further suggests that the use of recycled powder in sintered nylon part are ‘rescued’ with the addition of the virgin material.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.