Abstract
This paper describes the microstructural and mechanical properties of powder injection moulded (PIM) Ni based superalloys. Ni-based superalloys were mixed with a polymeric binder (paraffin wax, carnauba wax, stearic acid and PP) and injection moulded as standard tensile bars. The critical powder loading for injection moulding were 62.5 vol. % for standard samples. Binder removal, debinding, was performed using a two-step solvent/thermal method. After debinding the samples were sintered at 1100°C and at 1285°C under high level vacuum. Metallographic studies were conducted to reveal the extent of densification and the corresponding microstructural changes. Ni 718, Ni 625 and Nimonic90 samples achieved high sintered densities via supersolidus liquid phase sintering. The mechanical properties of Ni 718, Ni 625 and Nimonic90 are determined and compared with the properties of previously reported studies on similar PIM materials.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.