Abstract

This study examined the effect of blending poly(ethylene terephthalate) (PET) with 5% of a functionalized polymer. The blends were characterized by particle size and size distribution, unnotched tensile behavior, toughness, and notch sensitivity. The improved properties of blends that incorporated a functionalized elastomer were consistent with in situ formation of a graft copolymer by reaction with PET end groups. Triblock copolymers were examined that had styrene end blocks and an ethylene/butylene midblock (SEBS) with grafted maleic anhydride. The present study extended previous investigations that focused on level of grafting to examine the effects of component molecular weight and PET hydroxyl-to-carboxyl end-group ratio. Increasing the molecular weight of the SEBS and decreasing the hydroxyl-to-carboxyl ratio of the PET increased the effectiveness of the SEBS. In addition, a mix of an unfunctionalized SEBS with a functionalized SEBS was more effective than a single SEBS with the same total anhydride content. The same elastomers were the most effective for modifying a lower molecular weight PET (intrinsic viscosity 0.73) and a higher molecular weight PET (intrinsic viscosity 0.95). Some functionalized polypropylenes included in the study did not enhance the properties of PET. © 1999 John Wiley & Sons, Inc. J Appl Polym Sci 73: 203–219, 1999

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.