Abstract

Nowadays geopolymer concretes are subjected to heat curing. A large amount of highly corrosive and the hygroscopic alkaline activators are nowadays generally utilized in producing geopolymer concretes. In this paper, hybrid Ordinary Portland Cement (OPC) and geopolymer mixes are developed. The mainly used activator id the Solid potassium carbonate at different percentage is used as 5% & 10% of the weight of geopolymeric materials and OPC was blended with geopolymeric materials in different proportions. By adding cement, improves all the geopolymer properties except workability. By Applying external heat, it plays an important role in gaining strength. Strength gained by the absence of external heat is achieved by using Portland cement as a partial replacement of geocement. The influence of OPC content on the compressive strength development is investigated, and the optimized amount of solid activator to be used in the mix is also investigated. It is observed that percentage of strength increase decreases from52.24% to 14.77% as the OPC content increased from 20% to 60%.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.