Abstract
Porous thin films considered for applications like separation, sensing and microelectronic have to sustain mechanical stresses during their integration process or in working conditions. Thanks to recent progress in processing methods, it is now possible to precisely control the porosity and combine ordered mesopores with randomly-distributed macropores to achieve hierarchically porous materials. The mechanical properties of thin films containing different types of porosity (ordered meso, random macro and hierarchical) have been investigated by means of nanoindentation. In particular a method recently proposed by Li and Vlassak (H. Li, J.J. Vlassak, Journal of Materials Research 24 (2009) 1114–1126) is applied to account for the substrate effect. Residual indent impressions were imaged by Atomic Force Microscopy (AFM) to provide some insights in the mechanical behavior of the films. In addition, experimental indentation moduli are compared to theoretical predictions obtained via Finite Element (FE) analysis. The different porous structures have been modeled by FE to obtain the effective elastic properties from which the indentation modulus can be inferred. Finally, the experimental-model differences are discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have