Abstract

Commercially pure titanium (CP Ti), grade II, is subjected to hot compression at temperatures ranging from 673 to 973 K with 50 K intervals and strain rates of 0.001, 0.01, 0.1 and 1s-1 up to 60% height reduction. By analysing work hardening rate vs. flow stress, the deformation behaviour can be divided into three groups, viz. three-stage work hardening, two-stage work hardening and flow softening. By plotting the data in a T vs. logε diagram, the present and previous data fall into three distinct domains which can be separated by two distinct values of the Zener-Hollomon parameter.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.