Abstract

This paper is devoted to the study of the technological process for the production of tape from polyethylene and wood-polymer composite by extrusion. At the first stage, the wood-polymer composite granulate was obtained on a co-rotating twin-screw extruder. The tape was made on a Rheomex 19/25 PolyLab OS single-screw extruder with a barrel length L/D = 25. The processing temperature of the wood-polymer composite was in the range of 145 ... 160°C. The tensile strength and elasticity modulus in tension, water absorption per day and density were investigated for the developed wood-polymer composite and polyethylene. It has been found out that for the developed wood-polymer composite, the strength and elastic modulus along the stretch direction increase by 11% and 6%, respectively. Orientation stretching has a significant effect on the physical and mechanical properties of wood-polymer composites.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.