Abstract

Nanoindentation tests were conducted to investigate the near-surface mechanical properties of the individual components (fiber and matrix) for three-dimensional reinforced carbon/carbon composites (3D C/C). Optical microscope and polarizing light microscope were used to characterize the microstructure of 3D C/C. The microscopy results show that large number of pores and cracks exist at both bundle/matrix interface and pitch carbon matrix. These defects have important effect on the mechanical behavior of 3D C/C. The in situ properties for components of 3D C/C were acquired by nanoindentation technique. Relative to the matrix sample, the fiber samples have more larger values for modulus, stiffness and hardness. However, there is no significant difference of modulus and stiffness among fiber samples with different directions.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.