Abstract

The effect of natural rubber (NR) on mechanical, chemical and thermal properties of ground tire rubber (GTR) was investigated. Mechanical and thermal properties of GTR/NR vulcanized blends were determined with a universal testing machine and a dynamic mechanical analyzer (DMA). The molecular cross-linking density was determined by molecular swelling in toluene. Presents results indicate that the carbon black embedded in the GTR interior phase of the GTR/NR re-vulcanized blends, did not participate in the NR phase molecular motion restriction. The blends of GTR/NR showed the phenomenon known as reversion, leading a decreasing of the mechanical properties, that could be attributed of the degradation of the interphases (GTR/NR) n+j, j=1,2,3,…. On the other hand, the Cole-Cole charts of the GTR/NR vulcanized blends changed from a semicircular to an irregular form as the NR concentration increases, imposing the heterogeneity of the blend. In addition, in the Cole-Cole charts of GTR/NR vulcanized and re-vulcanized blends, the height ( E´´) and the width ( E´) of the curves decreased while the re-vulcanization processes number was greater; obtained results could be attributed to the increasing of the molecular cross-linking density.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.