Abstract

Studies on the mechanical properties and microstructures of as-cast and extruded Mg-Ce-Zn-Zr and Mg-Nd-Zn-Zr alloys have been made before and after heat treatment. The results show that the mechanical properties of as-cast Mg-Ce and Mg-Nd alloys are as good as those of typical die cast AZ91 alloy and the heat resistant WE43 alloy. In Nd-containing alloys, the precipitated phase Mg12 Nd contributes significantly to age hardening. The mechanical properties of extruded alloys are improved obviously compared with those of as-cast alloys. The ultimate strength is 257.8 MPa for extruded Mg-Ce alloy and 265.6 MPa for extruded Mg-Nd alloy. Extrusion is a useful method to improve both the strengths and elongations of the two experimental alloys at both ambient and elevated temperatures. The grain refinement and precipitation strengthening are the main strengthening mechanisms in the alloys. Tensile fracture surfaces show a dimple pattern after extruding and therefore reflect an improved elongation.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.