Abstract

Hybrid composites offer a combination of advantages of constituent components to produce a material with determined properties. In the present work, woven hybrid composite was prepared by hand lay-up method in laminate configuration. Kevlar/kenaf hybrid composites were fabricated with total fibre content of 30% and the ratio of Kevlar/kenaf varies in weight fraction of 78/22, 60/40, 50/50, 26/74, and 32/68, respectively. The Kevlar/epoxy and kenaf/epoxy were also prepared for comparison. The mechanical properties of hybrid, kenaf/epoxy, and Kevlar/epoxy composites were tested. Morphological properties of tensile fracture surface of hybrid composites were studied by scanning electron microscopy. Results have established that the mechanical properties of kenaf-Kevlar hybrid composites are a function of fibre content. The hybrid composites with Kevlar/kenaf (78/22) ratio exhibited better mechanical properties compared to other hybrid composites. This result indicates the potential of Kevlar-kenaf hybrid composite for impact applications.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call