Abstract : Silica xerogels have been prepared from tetraethylorthosilicate with 50 volume percent open porosity. Methyl methacrylate monomer has been introduced into xerogel monoliths and polymerized with ultraviolet radiation. The fully infiltrated silica gel - PMMA composite has a bulk density of about 1.6 g/cm cubed. The resulting composite is light-weight and optically transparent. Elastic constants have been determined with ultrasonics. Flexure strengths have been measured in 4-point bending. The flexure strength of the composite is over 100 MPa in comparison to 20 MPa for the silica xerogel. The composite is designed for use at or below room temperature.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.