In France, fission products are being vitrified for a possible final geological disposal. Under disposal conditions, corrosion of the glass by groundwater as well as stress corrosion because of stresses occurring at surface flaws cannot be excluded. Within this framework, the mechanical behavior of the French simulated nuclear waste glass SON68 was studied by Vickers indentation and fracture experiments in air and in a corrosive solution. The glass was corroded at 90°C in a solution enriched with Si, B, and Na. The results showed that the glass corrosion enhances the cracks propagation relative to experiments in air. The indentation fracture toughness (KIC) obtained using a four‐point bending test showed that the KIC of the glass decreased with increasing corrosion time.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.