Abstract
Geopolymers are amorphous to semi-crystalline with excellent physical and and mechanical properties. It has been used to become a potential binder to Ordinary Portland Cement (OPC) in certain applications due to its lower emission of carbon dioxide gases and low energy consumption sustainability criteria. Bottom Ash (BA) is one of the main industrial by-products and it is produced at the bottom of the furnace during the coal combustion process in electricity generation. The application of BA as a sustainable construction material in the building industry plays an important role in order to decrease the volume of residual waste and conserving existing natural fine aggregates. The objectives for this study is to study the effect of fly ash to bottom ash ratio and to determine the optimum ratio of fly ash to bottom ash geopolymer for pavement brick application. The chemical composition and morphology of geopolymer reinforcement was analysed by using X-ray Fluorescence and Scanning Electron Microscope. The molarity of the Sodium Hydroxide solution is fixed at 12M. The parameter used in this study are different weight percentage of fly ash geopolymer 0 wt%, 10 wt%, 20 wt%, 30 wt% and 40 wt%. The solid to liquid ratios for this study is 2.0. The curing temperature of this study is 80°C and the curing time is 24 hours. 100% of bottom ash geopolymer is used as a control variable for this study.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: IOP Conference Series: Materials Science and Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.