Abstract

The article aim is to analyze the influence of mechanical activation of a fly ash, with different proportion of mechanically activated and not mechanically activated material on alkali activation. The paper describes fly ash based geopolymers and their mechanical properties. Fly ashes were mixed in four different ratios with mechanically activated fly ash. Activation solution was constant in all specimens. Compressive and flexural strengths of the hardened product were tested after 7 and 28 days of the storage in laboratory conditions and samples were cured after activation in hot air chamber for 6 hours in 80°C temperature. The results show how mechanical activation of materials affects their strengths with highest amount achieved was 44 MPa.