Abstract

This paper simplifies a recently proposed method for measuring the thermal conductivity of powders using differential scanning calorimetry (DSC) (Sanchez-Rodriguez et al. in J Therm Anal Calorim 121:469–473, 2015). With this method, a crucible is filled with powder and a spherical metal reference is partially sunk into it. The thermal resistance between the metal and the crucible wall at the metal melting point is obtained from the DSC melting peak slope. In the simplified method outlined in this paper, a cylindrical pan is substituted for the original hemispherical crucible. The equivalence of both methods is demonstrated with alumina powder and commercial cylindrical crucibles of several sizes and aspect ratios.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.