Abstract

Methods for measuring the resistivity of materials during elastic and elastoplastic interactions of a current-conducting indenter and a studied sample are described. Analytical methods that describe the dependences of the contact ohmic resistance on the pressure force and the contact stiffness are proposed. The considered models are experimentally tested with a NanoScan scanning nanohardness tester using indenters made of boron-doped diamond single crystals.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.