Abstract
We report piezoresistance measurements of uniaxially strained graphene ribbons obtained by performing in-situ nanoindentation experiments on suspended graphene devices with simultaneous electrical measurements. We find the Young's modulus of graphene to be ~335 N/m, which is consistent with previous reports. We measure the gauge factor of graphene ribbons to be ~2, a value close to that predicted by a tight binding model.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.