Abstract
Strontium-doped lead zirconate titanate (PSZT) is reported to have a high piezoelectric coefficient (d33) in the range of 200−600 pm∕V, when in the form of ceramic disks or pellets. This article reports piezoelectric response results for PSZT thin films deposited by rf magnetron sputtering on gold-coated silicon substrates. The compositions of the deposited thin films have been found to be uniform with depth, using secondary ion mass spectroscopy. The surfaces of the deposited thin films have been studied using an atomic force microscope and observed to be regular and nanostructured in nature. The piezoelectric response of the thin films, using the inverse piezoelectric effect, has been measured using a nanoindenter. Values of thin film d33 up to 608 pm∕V were obtained, which is much higher than previously reported values of d33 for any thin film. The high values can be attributed to optimized deposition conditions and the low stress measured for the thin film arrangement on the substrate. The technique has been verified by obtaining a null response for silicon dioxide and by measuring d33 values of similar magnitude for PSZT thin films using an atomic force microscope in the same testing arrangement. The piezoelectric response has been mapped to study variations across the thin film and with distance from the top electrode.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.