Abstract
The purpose of this study was to investigate, in different experimental conditions, the galvanic corrosion phenomena which can exist between a dental suprastructure and a dental implant. The electrochemical behavior of 7 alloy superstructures with titanium and titanium alloy (Ti6Al4V) implants was investigated by electrochemical means in Fusayama–Meyer de-aerated saliva and Carter–Brugirard (AFNOR) non de-aerated saliva. Different techniques were used to obtain the value of the galvanic coupling current and potential for each couple. All showed very low corrosion rates, ranging from 10 -6 to 10 -8 A. Surface analysis confirmed these results.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.