Abstract

ABSTRACTThe chemical-vapor deposition conditions for the growth of pure boron (PureB) layers on silicon at temperatures as low as 400°C were investigated with the purpose of optimizing photodiodes fabricated with PureB anodes for minimal B-layer thickness, low dark current and chemical robustness. The B-deposition is performed in a commercially-available Si epitaxial reactor from a diborane precursor. In-situ methods commonly used to improve the cleanliness of the Si surface before deposition are tested for a deposition temperature of 450°C and PureB layer thickness of 3 nm. Specifically, high-temperature baking in hydrogen, and exposure to HCl are tested. Both material analysis and electrical diode characterization indicate that these extra cleaning steps degrade the properties of the PureB layer and the fabricated diodes.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.