Material flow and local texture evolution during friction stir spot welding (FSSW) of AZ31 magnesium alloy was characterized by varying tool rotation rates. Texture at various locations of the welded region was measured using electron backscatter diffraction (EBSD). Material flow is significantly influenced by tool rotation rate with a conical step spiral pin tool, and FSSW introduces a unique basal fiber texture in the welded region. Results indicate that local texture evolution is dominated by shear deformation through material flow. The tool shoulder applies both shear and compressive deformation to the upper region material; however, the rotating pin introduces only shear deformation to the adjacent material. As the tool rotation rate increases, the effect of both tool shoulder and pin becomes more prominent by introducing a higher degree of basal pole tilt with respect to the initial rolling texture at the periphery of the pin, but less tilt in the upper region beneath the tool shoulder undersurface. The equiaxed fine grain structure in the stir zone appears to result from the twinning-induced dynamic recrystallization and discontinuous dynamic recrystallization.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.