Abstract

Ti50Ni50, Ti50.5Ni49.5, Ti51Ni49 and Ti51.5Ni48.5 fibers were fabricated by melt overflow process. The rapid solidification can increase the solubility above the equilibrium solubility. The effects of the rapid solidification of Ti-rich Ti–Ni alloys on the microstructure, transformation temperatures and shape memory characteristics are investigated. The addition of 0.5at.% Ti in Ti50Ni50 alloy greatly increases the transformation temperature. However, the transformation temperatures decrease again for Ti content exceeding 51at.%. Results of thermal cycling tests under various constant stress levels reveal that the recoverable elongation associated with B2–B19 martensitic transformation of Ti50.5Ni49.5 fibers is two times larger than that of Ti51.5Ni48.5 alloy fiber.