Abstract
AbstractUnderstanding the finite volume throughout which plastic deformation begins is necessary to understand the mechanics of small-scale deformation. In indentation using spherical indenters, conventional yield criteria predict that yield starts at a point on the axis and at a depth of half the contact radius. However, Jayaweera et al (Proc. Roy. Soc. 2003)[4] concluded that yield occurs over a finite volume at least 100 nm thick. Semiconductor superlattice structures, in which the stress and thickness of individual layers can be varied and in which known internal stresses can be incorporated, open up new possibilities for investigation that cannot be achieved by varying external stresses on a homogenous specimen. We have designed samples with bands of highly strained InGaAs superlattice, which are essentially bands of low yield-stress material devoid of other metallurgical artifacts. These bands are placed at different depths in a series of samples. Spherical indenters with a range of radii were used to determine the elastic-plastic transition. The stress field from different sized indenters interacts with the low yield-stress material at different depths below the surface to map out the size of the initial yield volume.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.