Abstract

A Cu-36at.%In-15at.%Ga coating layer is manufactured using a warm spray process and ternary alloy powders. The powder used had a particle-size distribution of 5~22μm with a spherical shape and average particle size of 11.6μm. Pure aluminum plate was used as a substrate. As a result, a CIG coating layer with 120μm thickness was successfully obtained. In order to improve the density of the coating layer, post heat treatment was applied for 1 hour in each condition of 200, 300 and 400°C. Phase analysis of the powder initially used identified Cu9In4, Cu9Ga4 phases, and Cu9In4, Cu9Ga4, Cu3Ga phases were identified after warm spraying. As heat treatment was applied, porosity decreased from 0.98% (as sprayed) to 0.8% (400°C), showing an increase in density, and hardness also decreased from 304Hv (as sprayed) to 258Hv (400°C).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.