Abstract

The compressive deformation behavior in the thickness direction of a kinetic-sprayed pure-aluminum layer whose thickness is ~15 mm was investigated. The yield strength of coating material was 200 MPa, and a unique strain softening phenomenon occurred even at room temperature. Due to the initial severely deformed structure of the kinetic-sprayed coating material based on the results of microstructure analysis, the production of high-strength metal bulk materials using kinetic spray processes was deemed possible.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.