Abstract
In this paper, we use the High rate solidification to study process parameters and CMSX-6 super-alloy solidification structure. And then, it can provide more basis for the industrial directionally solidified casting of superalloys blades. The results show that: under certain process parameters, it can be obtained parallel columnar crystals directional solidification structure. The organization is composed of the matrix γ phase and the secondary precipitated γ ' phase; under an optical microscope, it can be observed the shrinkage porosity due to the volumes reduction arising solidification.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.