Abstract

It is well known that the CVD diamond films start to oxidize at temperatures above 700 °C, which may restrict their use in high temperature oxidation environment, such as for IR windows and cutting tools. Due to its high refractive index, the maximum transmission of diamond film is limited to approximately 71%. In the present investigation, HfO 2 and Y 2O 3 coatings were prepared by reactive magnetron sputtering of pure Hf and Y metal target in Ar + O 2 atmosphere. Adherent HfO 2 and Y 2O 3 coatings on high optical quality diamond film samples with optimum thickness for IR transmission enhancement in 8–12 µm and 3–5 µm were obtained. More than 20% increase in transmission was observed for both HfO 2/Diamond/HfO 2 and Y 2O 3/Diamond/Y 2O 3 coating systems. Excellent oxidation resistance for HfO 2/Diamond/HfO 2 and Y 2O 3/Diamond/Y 2O 3 coatings were demonstrated at temperatures up to 950 °C in oxidation environment.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.