Abstract
Thin films of granular metal and manganites ceramic were fabricated using RF magnetron sputtering and pulsed laser deposition techniques. The GMR effect is highly influenced by the shape, size and distribution of the magnetic entities. The highest GMR value of 7.6% for Ag/sub 87.0/Fe/sub 9.5/Co/sub 3.5/ granular film measured at 1 Tesla at room temperature had been obtained. In the polycrystalline manganites system, low-field magnetoresistance (LFMR) had been observed due to the grain boundaries. LFMR of 4.3% and 6.2% measured at 0.1 Tesla at room temperature have been observed for both La-Sr-Mn-O and La-Ba-Mn-O samples. For the La-Sr-Mn-O film, LFMR ratio of 4.5% has been observed. This value meets the requirement as sensor element and it is currently used in many applications such as head sensing in hard disk.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.