Abstract

A direct comparison between the surface and the bulk hysteretic behavior of particulate oxide recording media was made for the first time. The surface properties were measured using a magneto-optic Kerr effect apparatus operating in fields up to 10 kOe while the bulk hysteresis loops were measured with a vibrating sample magnetometer. Because of the very small Kerr rotations observed, typically an order of magnitude less than those of metal films, careful attention to experimental detail was required. Several different types of particulate recording media were measured. The surface coercivity was found to be about 10% higher than the bulk coercivity for some of the high energy tapes; however, it was virtually identical to the bulk coercivity in several other samples. A thorough discussion of the apparatus is given.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.