Abstract

The crack formation in filaments of multi-filamentary Bi 2Sr 2Ca 2Cu 3O x tapes as function of applied longitudinal strain is visualized by means of magneto-optical imaging. Strain is applied at the desired temperature inside a helium flow cryostat. Cracks form transverse to the current carrying direction of the filaments. Before the tape breaks entirely, all filaments have formed a large number of transverse cracks, spaced with an average crack distance of ≈200 μm. The crack formation is compared with the degradation of the critical current as a function of the applied strain. The critical current degrades already before the first crack is observed. This is explained by the limited number of filaments visible in the experiment.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.