Abstract
Magnetization AC loss measurements of singe- and seven-core Ba122/Ag tapes have been done by calibration-free method in the range of temperature from 20 K to 42 K and field magnitudes up to 70 mT in RMS with two frequencies 72 Hz and 144 Hz. A strong effect of eddy current losses in highly conductive Ag sheath was observed for single-core sample, but negligible for seven-core tape with more resistive AgSn alloy outer sheath. For the estimation of eddy current loss component, pure Ag foil was measured in the same range of temperatures and used for analytical subtraction from the total losses of Ba122/Ag. In addition, loss measurement of singe-core sample with chemically etched away Ag sheath was also done. AC loss measurements in perpendicular as well as parallel field orientation have shown a strong effect of the filament size.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.