The magnetic susceptibility χ of coarse-grained WC and nanocrystalline n-WC tungsten carbides has been studied in a temperature range of 300–1250 K. The dependence χ (T) for coarse-grained WC carbide has no singularities. A stable particle size of about 55 nm remains in the n-WC nanopowder after annealing at 300–1200 K, whereas the relaxation of microstrains occurs at 550–920 K. The dependence χ(T) for nanocrystalline n-WC carbide in a range of 550–920 K exhibits features associated with the annealing of microstrains, which reduces the contribution of orbital paramagnetism to the susceptibility of n-WC carbide and initiates the precipitation of small iron and cobalt impurities in the form of superparamagnetic particles.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.